Polymaker概览
Polymaker是来自中国的耗材品牌,在开放耗材数据库中有61个耗材系列:PLA, PC, PETG, PVA, PA6和ABS。
热门Polymaker耗材
SimplyPrint账户最常用的Polymaker产品系列,使用最多的排在前面。
所有Polymaker耗材
PLA (36)
PC (5)
PETG (4)
PVA (4)
PA6 (3)
ABS (2)
TPU (2)
ASA (1)
CPE (1)
PA12 (1)
PET (1)
PVB (1)
Polymaker耗材打印设置
每种Polymaker耗材的喷嘴和打印床温度,采用Polymaker在开放耗材数据库中提供的数据;如未提供,则采用其切片软件配置中的数据。
| 耗材 | 材料 | 喷嘴 | 打印床 | 颜色 |
|---|---|---|---|---|
| Army Panchroma Matte PLA | PLA | 190-230 °C | 50-70 °C | 6 |
| Celestial Panchroma PLA | PLA | 190-230 °C | 50-70 °C | 3 |
| Draft PLA | PLA | 190-230 °C | 25-61 °C | 1 |
| Galaxy Panchroma PLA | PLA | 190-230 °C | 50-70 °C | 5 |
| Gradient Panchroma Matte PLA | PLA | 190-230 °C | 50-70 °C | 7 |
| Gradient Panchroma PLA | PLA | 190-230 °C | 25-61 °C | 2 |
| HT-PLA | PLA | 210-230 °C | 25-61 °C | 14 |
| HT-PLA-GF | PLA | 210-230 °C | 25-61 °C | 9 |
| LW PolyLite PLA | PLA | 190-210 °C | 25-61 °C | 7 |
| Marble Panchroma PLA | PLA | 190-230 °C | 50-70 °C | 5 |
| Matte PLA | PLA | 190-230 °C | 50-70 °C | 2 |
| PLA | PLA | 190-230 °C | 50-70 °C | 4 |
| Panchroma Glow PLA | PLA | 190-230 °C | 25-61 °C | 8 |
| Panchroma Matte PLA | PLA | 190-230 °C | 50-70 °C | 19 |
| Panchroma PLA | PLA | 190-230 °C | 25-61 °C | 4 |
| Panchroma Silk PLA | PLA | 190-230 °C | 25-61 °C | 34 |
| Pastel Panchroma Matte PLA | PLA | 190-230 °C | 50-70 °C | 8 |
| Polylite PLA | PLA | 190-230 °C | 25-61 °C | 39 |
| Polymaker™ PLA Pro | PLA | 210-230 °C | 30-60 °C | 32 |
| Starlight Panchroma PLA | PLA | 190-230 °C | 50-70 °C | 9 |
| Translucent Panchroma PLA | PLA | 190-230 °C | 50-70 °C | 5 |
| Creator Special Edition PLA | PLA | 190-230 °C | 50-70 °C | 3 |
| Dual Panchroma Matte PLA | PLA | 190-230 °C | 25-61 °C | 11 |
| For Production Matte PLA | PLA | 190-230 °C | 50-70 °C | 2 |
| Metallic Panchroma PLA | PLA | 190-230 °C | 50-70 °C | 3 |
| Metallic PolyLite PLA | PLA | 190-230 °C | 50-70 °C | 6 |
| Metallic Polylite Silk PLA | PLA | 190-230 °C | 50-70 °C | 2 |
| Muted Panchroma Matte PLA | PLA | 190-230 °C | 25-61 °C | 5 |
| Neon Panchroma PLA | PLA | 190-230 °C | 25-61 °C | 6 |
| PLA PolyCast | PLA | 190-220 °C | 25-71 °C | 1 |
| PLA PolySmooth | PLA | 190-220 °C | 25-71 °C | 4 |
| PolyMax™ PLA | PLA | 190-230 °C | 25-61 °C | 12 |
| Polylite PLA CF | PLA | 190-230 °C | 25-61 °C | 1 |
| Polysonic PLA | PLA | 190-230 °C | 50-70 °C | 10 |
| Satin Panchroma PLA | PLA | 190-230 °C | 25-61 °C | 8 |
| Temp Shift Panchroma PLA | PLA | 190-230 °C | 50-70 °C | 2 |
| PC-ABS | PC | 250-270 °C | 90-106 °C | 2 |
| Polylite PC | PC | 250-270 °C | 90-106 °C | 1 |
| PC | PC | 260-300 °C | 100-120 °C | 2 |
| PC-PBT | PC | 260-280 °C | 100-116 °C | 2 |
| Polymax PC | PC | 250-270 °C | 90-106 °C | 7 |
| PETG | PETG | 240-260 °C | 60-70 °C | 21 |
| Polylite PETG | PETG | 230-260 °C | 70-80 °C | 24 |
| PETG CF | PETG | 220-250 °C | 70-90 °C | 1 |
| Polymax PETG | PETG | 230-260 °C | 70-80 °C | 2 |
| PolySupport for PLA | PVA | 220-230 °C | 25-61 °C | 1 |
| PVA | PVA | 180-210 °C | 50-60 °C | 1 |
| PVA PolyDissolve S1 | PVA | 215-225 °C | 25-61 °C | 1 |
| PVA PolySupport for PA12 | PVA | 270-300 °C | 50-80 °C | 1 |
| PA6 CF | PA6 | 250-290 °C | 80-100 °C | 1 |
| Polymide Copa PA6 | PA6 | 250-270 °C | 25-51 °C | 2 |
| PA6 GF | PA6 | 250-290 °C | 80-100 °C | 1 |
| Polylite ABS | ABS | 245-265 °C | 90-100 °C | 26 |
| Metallic Polylite Silk ABS | ABS | 230-260 °C | 90-110 °C | 2 |
| Polyflex 95 Hf High Speed TPU | TPU | 200-230 °C | 25-51 °C | 3 |
| Polyflex TPU | TPU | 210-240 °C | 30-60 °C | 11 |
| Polylite ASA | ASA | 230-260 °C | 75-95 °C | 25 |
| Panchroma CPE | CPE | 240-270 °C | 70-90 °C | 27 |
| PA12 CF | PA12 | 240-270 °C | 80-100 °C | 1 |
| PET CF | PET | 220-250 °C | 70-90 °C | 1 |
| PolySmooth | PVB | 190-220 °C | 25-71 °C | 10 |
Polymaker料盘和NFC标签
SimplyPrint可为任何Polymaker料盘写入标签,使其像系统制造商自有的料盘一样使用:
SimplyPrint账户中的Polymaker
来自SimplyPrint账户的料卷,汇总统计截至23 Oct 2026。无法识别任何账户。
- 使用
- 100+个账户
- 打印农场
- 由多个SimplyPrint用户使用
- 企业
- 由多个SimplyPrint用户使用
- 学校和大学
- 由多个SimplyPrint用户使用
- 业余爱好者
- 100+个账户
常见问题
打印PolymakerPLA时应使用什么温度?
根据系列不同,Polymaker的PLA系列建议喷嘴温度为190-230 °C,热床温度为25-71 °C。各系列页面均提供准确范围和切片软件配置文件。
打印PolymakerPC时应使用什么温度?
根据系列不同,Polymaker的PC系列建议喷嘴温度为250-300 °C,热床温度为90-120 °C。各系列页面均提供准确范围和切片软件配置文件。
Polymaker耗材来自哪里?
Polymaker是来自中国的品牌。其耗材的生产地可能不同,开放耗材数据库记录的是该品牌所在国家。
Polymaker耗材有RFID或NFC标签吗?
据我们所知,没有。SimplyPrint可为任何Polymaker线轴写入适用于Creality CFS, Anycubic ACE, OpenPrintTag, ELEGOO Canvas, OpenSpool, QidiTech, OpenTag和TigerTag的标签。
在哪里购买Polymaker耗材?
来自Polymaker自营商店,以及每种耗材页面上的其他商店,按您所在地区筛选。
Polymaker生产哪些耗材?
PLA, PC, PETG, PVA, PA6, ABS, TPU, ASA, CPE, PA12, PET和PVB。